Abstract

This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of a type of resin-matrix composites, carbon-epoxy composites. The fractographs illustrate the fracture modes found in composite prepregs, composite panels, solid rocket motor nozzles, and tension, flexural, compressive, and shear loadings.