This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of pearlitic malleable and ferritic malleable white irons, and in identifying and interpreting the morphology of fracture surfaces. The fractographs illustrate the fracture sequence, localized plastic deformation, and microcrack initiation and propagation of these irons.