Welding codes and standards usually require the qualification of welding procedures prior to being used in production. This is to ensure that welds will meet the minimum quality and mechanical property requirements for the application. This article provides an overview of the welding procedure qualification guidelines and test methods. It also reviews the codes, standards, and specifications that govern the design and fabrication of welded structures for the procedure qualification details that are appropriate for a given application.