Skip to Main Content
ASM Handbook

Welding, Brazing and Soldering

Edited by
David LeRoy Olson
David LeRoy Olson
Search for other works by this author on:
;
Thomas A. Siewert
Thomas A. Siewert
Search for other works by this author on:
;
Stephen Liu
Stephen Liu
Search for other works by this author on:
;
Glen R. Edwards
Glen R. Edwards
Search for other works by this author on:
ASM International
Volume
6
ISBN electronic:
978-1-62708-173-3
Publication date:
1993
Book Chapter

Introduction to Solid-State Welding

By
Ray Dixon
Ray Dixon
Los Alamos National Laboratory
Search for other works by this author on:
Published:
1993
Page range:
141 - 142

Abstract

Solid-state welding (SSW) processes are those that produce coalescence of the faying surfaces at temperatures below the melting point of the base metal being joined without the addition of brazing or solder filler metal. This article discusses the fundamentals of welding and joining materials via the application of a nonmelting process. The specific processes usually associated with the nonmelting process are discussed.

You do not currently have access to this content.
Don't already have an account? Register

Ray Dixon, 1993. "Introduction to Solid-State Welding", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal