Skip to Main Content
ASM Handbook

Welding, Brazing and Soldering

Edited by
David LeRoy Olson
David LeRoy Olson
Search for other works by this author on:
;
Thomas A. Siewert
Thomas A. Siewert
Search for other works by this author on:
;
Stephen Liu
Stephen Liu
Search for other works by this author on:
;
Glen R. Edwards
Glen R. Edwards
Search for other works by this author on:
ASM International
Volume
6
ISBN electronic:
978-1-62708-173-3
Publication date:
1993
Book Chapter

Resistance Spot Welding[1]

By
Neville T. Williams
Neville T. Williams
British Steel
Search for other works by this author on:
Published:
1993
Page range:
226 - 229

Abstract

Resistance spot welding (RSW) is a process in which faying surfaces are joined in one or more spots by the heat generated by resistance to the flow of electric current through workpieces that are held together under force by electrodes. This article discusses the major advantages of spot welding and the three principal elements, such as electrical circuit, control circuit, and mechanical system, of RSW machines. It reviews the three basic types of RSW machines: pedestal-type welding machines, portable welding guns, and multiple spot welding machines. The article provides information on weldabilily of uncoated steels and zinc-coated steels, as well as aluminum alloys.

You do not currently have access to this content.
Don't already have an account? Register

Neville T. Williams, 1993. "Resistance Spot Welding", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal