Abstract

The effective integration of aluminum metal-matrix composites (Al-MMCs) into useful structures and devices often requires an understanding of the weldability of Al-MMCs that includes a thorough knowledge on the effects of various interactions between matrix and reinforcement. This article provides a detailed discussion on weldability and the effect of viscosity, chemical reactions, and solidification on weldability. It discusses different welding processes, namely, gas-tungsten arc welding, gas-metal arc welding, laser-beam welding, electron-beam welding, resistance welding, friction welding, transient liquid phase bonding, and capacitor discharge welding.

You do not currently have access to this chapter.
Don't already have an account? Register

Thomas J. Lienert, Charles T. Lane, Jerry E. Gould, 1993. "Selection and Weldability of Aluminum Metal-Matrix Composites", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal