The selection of materials for welded construction applications involves a number of considerations, including design codes and specifications. Mobile structures have quite different materials requirements for weight, durability, and safety than stationary structures, which are built to last for many years. This article provides an overview of the service conditions. It offers guidance for material selection applications, including bridges and buildings, pressure vessels and piping, shipbuilding and offshore structures, aerospace systems, machinery and equipment, automobiles, railroad systems, and sheet metal. Material properties and welding processes that may be significant in meeting design goals are also described.

You do not currently have access to this chapter.
Don't already have an account? Register

ASM Committee on Material Requirements for Service Conditions , R. David Thomas, Jr., Bruno L. Alia, William R. Apblett, Robert G. Bartifay, Stephen A. Coughlin, Gregory Melekian, Anthony R. Mellini, Sr., Larry Perkins, James E. Roth, William J. Ruprecht, Bernard E. Schaltenbrand, Robert E. Somers, Roger K. Steele, 1993. "Material Requirements for Service Conditions", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal