This article describes resistivity effects and Curie temperature effects on coupling efficiency during induction heating in the soldering operation. It discusses the effects of workpiece geometry during the induction heating. The practices associated with the use of preplaced solder are reviewed. The article provides useful information on setup parameters and safety concerns for the use of induction heating.

You do not currently have access to this chapter.
Don't already have an account? Register

Paul T. Vianco, 1993. "Induction Soldering", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards