Abstract

This article reviews quantifying adhesion, bonding, and interfacial characterization and strength in a solid-state welding process. It discusses metal-metal configurations and provides information on experimental work carried out in measuring the mechanical properties of interfaces based on theoretical analysis. A discussion on the properties affecting adhesion is also provided.

You do not currently have access to this chapter.
Don't already have an account? Register

Ray Dixon, S.P. Chen, 1993. "Fundamentals of Metal and Metal-to-Ceramic Adhesion", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards