Skip to Main Content

Abstract

This article presents in-depth metallurgical information about the response of carbon and low-alloy steels to welding conditions and micro-structural evolution in the weld heat-affected zone. It discusses the fabrication weldability and service weldability of carbon and low-alloy steels. The article describes six general classes of the metal: low-carbon steels, high-strength low-alloy steels, quenched-and-tempered steels, heat-treatable low-alloy steels, thermal-mechanical-controlled processing steels, and chromium-molybdenum steels. It concludes with an illustration of steels' susceptibility to hydrogen-assisted cold cracking relative to carbon content and carbon equivalent.

Abstract

This article describes the common defects associated with arc welds in the weld metal and the heat-affected zone (HAZ) of the plate. These defects include porosity, incomplete fusion, hot cracks, lamellar tearing, undercut, rollover, and inclusions. The article details hydrogen-induced cracking and its mechanism as well as the control measures. It provides information on measurement of hydrogen in weld metal and presents a table that contain information on effect of welding processes and electrodes on hydrogen levels in welds.

You do not currently have access to this chapter.
Don't already have an account? Register

Bruce R. Somers, 1993. "Selection of Carbon and Low-Alloy Steels", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal