Book Chapter
Postweld Heat Treatment of Nonferrous High-Temperature Materials
By
Steven C. Ernst
Steven C. Ernst
Haynes International, Inc.
Search for other works by this author on:
-
Published:1993
Abstract
This article provides an overview of the types of postweld heat treatment processes carried out in solid-solution-strengthened and precipitation-strengthened nonferrous high-temperature nickel and cobalt alloys.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Steven C. Ernst, Postweld Heat Treatment of Nonferrous High-Temperature Materials, Welding, Brazing and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 572–574, https://doi.org/10.31399/asm.hb.v06.a0001424
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.
Related Book Content
General Welding Characteristics of High-Temperature Materials
Welding, Brazing and Soldering
Welding Metallurgy of Nonferrous High-Temperature Materials
Welding, Brazing and Soldering
Repair Welding of Castings
Casting
Flash Welding and Upset Welding
Welding Fundamentals and Processes
Preheat and Postweld Heat Treatment Temperatures for Selected Steels
Welding Fundamentals and Processes
Selection of Nickel-Base Corrosion-Resistant Alloys Containing Molybdenum
Welding, Brazing and Soldering
Welding of Cast Irons
Welding, Brazing and Soldering