Welding, Brazing and Soldering
Abstract
This article provides information on the base material properties of wrought duplex stainless steels (DSS). These properties include microstructure, alloy grades, mechanical and physical properties, and corrosion resistance. The article reviews the applications and microstructural development of DSS. It describes the factors influencing welding and weldability of the DSS. These factors include preheating, postweld heat treatment, interpass temperature control, welding practices, welding procedure qualification, filler metal requirements, cracking behavior, and loss of properties. The article examines the applicable welding processes such as fusion welding and solid-state welding processes.
Sign in
ASM members
Member Sign InDavid N. Noble, Selection of Wrought Duplex Stainless Steels, Welding, Brazing and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 471–481, https://doi.org/10.31399/asm.hb.v06.a0001411
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.