Welding, Brazing and Soldering
Validation Strategies for Heat-Affected Zone and Fluid-Flow Calculations
-
Published:1993
Abstract
Fusion welding processes involve four phase changes, namely, solid-solid state, solid-liquid, liquid-vapor, and vapor-plasma. Each has its own thermal, momentum, and stress history. This article discusses some important techniques to validate temperature, momentum, stress, and residual strain history observed in the heat-affected zone of fusion welded materials.
Sign in
ASM members
Member Sign InJ. Mazumde, Validation Strategies for Heat-Affected Zone and Fluid-Flow Calculations, Welding, Brazing and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 1147–1152, https://doi.org/10.31399/asm.hb.v06.a0001482