Selection and Weldability of Advanced Titanium-Base Alloys
By
David H. Phillips
David H. Phillips
Edison Welding Institute
Search for other works by this author on:
-
Published:1993
Abstract
This article focuses on the physical metallurgy and weldability of four families of titanium-base alloys, namely, near-alpha alloy, alpha-beta alloy, near-beta, or metastable-beta alloy, and titanium based intermetallics that include alpha-2, gamma, and orthorhombic systems.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
David H. Phillips, Selection and Weldability of Advanced Titanium-Base Alloys, Welding, Brazing and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 524–527, https://doi.org/10.31399/asm.hb.v06.a0001416
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.
Related Book Content
Selection and Weldability of Conventional Titanium Alloys
Welding, Brazing and Soldering
Effect of Heat Treatment on Mechanical Properties of Titanium Alloys
Heat Treating of Nonferrous Alloys
Welding Metallurgy of Nonferrous High-Temperature Materials
Welding, Brazing and Soldering
Solid-State Transformations in Weldments
Welding Fundamentals and Processes
Introduction to Bulk-Forming Processes
Metalworking: Bulk Forming
Corrosion Resistance of Titanium Alloys
Corrosion: Fundamentals, Testing, and Protection
Selection of Cast Stainless Steels
Welding, Brazing and Soldering
Selection and Weldability of Heat-Treatable Aluminum Alloys
Welding, Brazing and Soldering
Selection and Weldability of Non-Heat-Treatable Aluminum Alloys
Welding, Brazing and Soldering
Selection of Wrought Duplex Stainless Steels
Welding, Brazing and Soldering