This article emphasizes the physical metallurgy of titanium and titanium alloys along with their microstructural response to fusion welding condition. The titanium alloys are classified into unalloyed or commercially pure titanium, alpha and near-alpha alloys, alpha-beta alloys, and metastable beta alloys. The article further discusses the weld microstructure for alpha-beta and metastable beta alloys and describes welding defects observed in titanium alloys. The influence of macro- and microstructural characteristics of titanium weldment on mechanical properties is also discussed. The article concludes with a discussion on the different welding processes used in the welding of titanium and titanium alloys.

You do not currently have access to this chapter.
Don't already have an account? Register

W.A. Baeslack, III, J.R. Davis, C.E. Cross, Selection and Weldability of Conventional Titanium Alloys, Welding, Brazing and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 507–523, https://doi.org/10.31399/asm.hb.v06.a0001415

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal