This article describes the dip brazing process and the principal types of furnaces used for molten-salt-bath dip-brazing applications. It provides information on equipment maintenance, which is divided into temperature control, control of the liquid, and maintenance of the vessel. The article presents the typical salts used for molten-salt dip brazing of carbon and low-alloy steels with selected filler metals in tabular form. It concludes with information on dip brazing of stainless steels, cast irons, and aluminum alloys and safety precautions of the process.

You do not currently have access to this chapter.
Don't already have an account? Register

Daryl D. Peter, Dip Brazing, Welding, Brazing and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 336–338, https://doi.org/10.31399/asm.hb.v06.a0001388

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal