Electron-beam welding (EBW) can produce deep, narrow, and almost parallel-sided welds with low total heat input and relatively narrow heat-affected zones in a wide variety of common and exotic metals. This article discusses the joint configurations and shrinkage stresses encountered in various joint designs for electron-beam welding, as well as special joints and welds including multiple-pass welds, tangent-tube welds, three-piece welds, and multiple-tier welds. It provides a comparison of medium vacuum EBW with high-vacuum EBW. Scanning is a method of checking the run-out between the beam spot and the joint to be welded. The article describes various scanning techniques for welding dissimilar metals and provides information on the application of electron-beam wire-feed process for repairs. It concludes with a discussion on EBW of heat-resistant alloys, refractory metals, aluminum alloys, titanium alloys, copper and copper alloys, magnesium alloys, and beryllium.

You do not currently have access to this chapter.
Don't already have an account? Register
Close Modal

or Create an Account

Close Modal
Close Modal