Upset Welding[1]
-
Published:1993
Abstract
Upset welding (UW) is a resistance welding process utilizing both heat and deformation to form a weld. A wide variety of shapes and materials can be joined using upset welding in either a single-pulse or continuous mode. This article discusses the advantages and disadvantages of upset welding, as well as the types of welds. The advantages include speed, ease of control, fewer defects, enhanced weld properties, simplicity of equipment, less-strict composition requirements, and ability to join difficult-to-weld materials. The article reviews the role of a homopolar generator as an alternative method for supplying the electrical current for upset welding.
Sign in
ASM members
Member Sign InW.R. Kanne, Jr., 1993. "Upset Welding", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards
Download citation file:
Close
ASM Reference Publications Catalog
The new Fall / Winter 2019-2020 Catalog features more than 200 new and upcoming releases and our popular best-selling titles. Save now with prepublication pricing and set sales.