Abstract
Vapor-phase soldering is a process of condensation heating in which the product prepared for soldering is passed through or into a layer of saturated vapor. This article provides an overview of the soldering process with emphasis on its applications and the equipment used.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Dale L. Linman, Vapor-Phase Soldering, Welding, Brazing and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 369–370, https://doi.org/10.31399/asm.hb.v06.a0001402
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.
Related Topics
Related Book Content
Dip Soldering
Welding, Brazing and Soldering
Resistance Soldering
Welding, Brazing and Soldering
Torch Soldering
Welding, Brazing and Soldering