During fusion welding, the thermal cycles produced by the moving heat source cause physical state changes, metallurgical phase transformation, and transient thermal stress and metal movement. This article presents an analysis of heat flow in the fusion welding process. The primary objective of welding heat flow modeling is to provide a mathematical tool for thermal data analysis, design iterations, or the systematic investigation of the thermal characteristics of any welding parameters. The article addresses analytical heat-flow solutions and their practical applications. It describes the effects of material property and welding condition on the temperature distribution of weldments. The thermal properties of selected engineering materials are provided in a table.

You do not currently have access to this chapter.
Don't already have an account? Register

Chon L. Tsai, Chin M. Tso, Heat Flow in Fusion Welding, Welding, Brazing and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 7–18, https://doi.org/10.31399/asm.hb.v06.a0001333

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal