This article discusses the weldability characteristics of cobalt-base corrosion-resistant (CR) alloys, titanium-base CR alloys, zirconium-base CR alloys, and tantalum-base CR alloys that assist in the selection of suitable alloy and welding method for producing high-quality welds.

You do not currently have access to this chapter.
Don't already have an account? Register

S.J. Matthews, Selection of Cobalt-, Titanium-, Zirconium-, and Tantalum-Base Corrosion-Resistant Alloys, Welding, Brazing and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 598–600, https://doi.org/10.31399/asm.hb.v06.a0001430