This article commences with a brief description of the solidification characteristics and microstructures of martensitic precipitation hardening (PH) stainless steels. It reviews the welding parameters for types 17-4PH, 15-5PH, PH13-8 Mo, Custom 450, and Custom 455. The article describes the microstructural evolution and weld parameters associated with semiaustenitic PH steels. It discusses the weldability and welding recommendations for A-286 and JBK-75 austenitic PH stainless steels. The article also presents tables that list properties and heat treatments for the PH stainless steels.