Welding, Brazing and Soldering
Abstract
This article reviews quantifying adhesion, bonding, and interfacial characterization and strength in a solid-state welding process. It discusses metal-metal configurations and provides information on experimental work carried out in measuring the mechanical properties of interfaces based on theoretical analysis. A discussion on the properties affecting adhesion is also provided.
Sign in
ASM members
Member Sign InRay Dixon, S.P. Chen, Fundamentals of Metal and Metal-to-Ceramic Adhesion, Welding, Brazing and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 143–149, https://doi.org/10.31399/asm.hb.v06.a0001348