This article discusses the susceptibility of carbon steels to hydrogen-induced cracking, solidification cracking, lamellar tearing, weld metal porosity, and heat-affected zone (HAZ) mechanical property variations. The composition and mechanical properties of selected carbon steels used in arc welding applications are listed in a table. The article presents process selection guidelines for arc welding carbon steels. It provides information on the shielded metal arc welding, gas-metal arc welding, and flux-cored arc welding, gas-tungsten arc and plasma arc welding, submerged arc welding, electrogas welding, electroslag welding, and stud arc welding.

This article discusses factors involved in selecting welding processes and...