Abstract

Compression molding is the single largest primary manufacturing process used for automotive composite applications. This article provides a general overview of the compression molding process. It describes the basic design, materials, and processing equipment of three main groups of composite materials, namely, glass-fiber-mat-reinforced thermoplastics, long-fiber-reinforced thermoplastics, and sheet molding compounds. It presents information on the application examples and market volume of compression molding.

You do not currently have access to this chapter.
Don't already have an account? Register

Charles W. Peterson, G. Ehnert, R. Liebold, K. Hörsting, R. Kühfusz, 2001. "Compression Molding", Composites, Daniel B. Miracle, Steven L. Donaldson