Skip to Main Content
ASM Handbook

Composites

Edited by
Daniel B. Miracle
Daniel B. Miracle
Search for other works by this author on:
;
Steven L. Donaldson
Steven L. Donaldson
Search for other works by this author on:
ASM International
Volume
21
ISBN electronic:
978-1-62708-195-5
Publication date:
2001
Book Chapter

Post-Processing and Assembly of Ceramic-Matrix Composites

By
David Lewis, III
David Lewis, III
Naval Research Laboratory
Search for other works by this author on:
;
M. Singh
M. Singh
QSS Group, Inc., NASA Glenn Research Center
Search for other works by this author on:
Published:
2001
Page range:
668 - 673
Publication history
November 01, 2001

Abstract

Post-processing includes various processes that might be required to produce finished components from the ceramic-matrix composites (CMC) materials. The processes include machining or finishing operations, coating, joining, assembly operations, and nondestructive evaluation of CMCs and its components. This article discusses the specific needs for science and technology in these areas relative to the goal of employing CMCs in a variety of applications.

You do not currently have access to this content.
Don't already have an account? Register

David Lewis, III, M. Singh, 2001. "Post-Processing and Assembly of Ceramic-Matrix Composites", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal