Abstract

Interpretation of failures of ceramic-matrix composites, and in particular continuous fiber reinforced ceramic-matrix composites is complicated by the complex structure of the composite material. This article describes the failure characteristics and evidence of failure mechanisms of these composites, with illustrations.

You do not currently have access to this chapter.
Don't already have an account? Register

Michael G. Jenkins, Raj N. Singh, 2001. "Failure Analysis of Ceramic-Matrix Composites", Composites, Daniel B. Miracle, Steven L. Donaldson