Good hole-drilling processes are key to joining composite parts with other composite parts or with metal parts. This article discusses the considerations for drilling polymer-matrix composites. It describes the use of power-feed drill motors and automated drilling/fastener installation equipment. The article provides a discussion on reaming, countersinking, and three recommended choices of cutting tools for producing a countersink in carbon/epoxy structure. The cutting tools include: standard carbide insert cutters, solid carbide cutters, or polycrystalline diamond (PCD) insert cutters. The article concludes with a discussion on inspection of hole quality.

You do not currently have access to this chapter.
Don't already have an account? Register

Michael J. Paleen, Jeffrey J. Kilwin, 2001. "Hole Drilling in Polymer-Matrix Composites", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal