Abstract

This article focuses on the unique characteristics of composites and laminated plates, including orthotropic, anisotropic, and unsymmetric plates. It discusses stability issues associated with practical, structural laminates based on the finite stack effects and transverse shear stiffness effects. The article presents the study of instability associated with postbuckling behavior and hygrothermal buckling in composite sandwich panels and shell panels.

You do not currently have access to this chapter.
Don't already have an account? Register

Gerald Flanagan, Carol Meyers, 2001. "Instability Considerations", Composites, Daniel B. Miracle, Steven L. Donaldson