This article provides information on the classification of various composites manufacturing processes based on similar transport processes. The composites manufacturing processes can be grouped into three categories: Short-fiber suspension methods, squeeze flow methods, and porous media methods. The article presents an overview of modeling philosophy and approach that is useful in describing the composites manufacturing processes.