Composite materials offer amazing opportunities for delivering structures that are optimized to meet design requirements. This article provides a summary of the concepts discussed in the articles under the section “Engineering Mechanics, Analysis, and Design” in ASM Handbook, Volume 21: Composites. The section introduces many of the engineering approaches used in composite industry.