Abstract

This article discusses the three basic elements of an epoxy resin formulation that must be understood when selecting a thermoset system. These include base resins, epoxy resin curatives, and modifiers. The article provides examples of epoxy resin formulations that illustrate how raw materials are combined to tailor a formulation to a specific application. It concludes with a discussion on general guidelines for the safe handling of epoxy resins and their associated products.

You do not currently have access to this chapter.
Don't already have an account? Register

Maureen A. Boyle, Cary J. Martin, John D. Neuner, 2001. "Epoxy Resins", Composites, Daniel B. Miracle, Steven L. Donaldson