This article describes the machining operations of carbon fiber-reinforced epoxy, or carbon/epoxy thermoset composite materials, such as drilling, reaming, routing, trimming, end milling, slot milling, and facing. It reviews cutting tools for machining, including solid carbide, diamond plated, brazed diamond, diamond coated carbide, and polycrystalline cutting tools. The article also describes cutting tool materials that are used for peripheral milling, face milling, and the trimming of polymer-matrix composites.