Abstract

This article provides information on the applications of fiber-reinforced composites in commercial and military aircrafts. It tabulates the composite components in various types of aircraft. The applications of the composites in the components of Boeing 727, 737, 757, 767, 777, and 777-200 are schematically illustrated.