Skip to Main Content
ASM Handbook

Composites

Edited by
Daniel B. Miracle
Daniel B. Miracle
Search for other works by this author on:
;
Steven L. Donaldson
Steven L. Donaldson
Search for other works by this author on:
ASM International
Volume
21
ISBN electronic:
978-1-62708-195-5
Publication date:
2001
Book Chapter

High-Temperature Applications

By
Tito T. Serafini
Tito T. Serafini
General Electric Aircraft Engines
Search for other works by this author on:
;
Stephen C. Mitchell
Stephen C. Mitchell
General Electric Aircraft Engines
Search for other works by this author on:
Published:
2001
Page range:
1050 - 1056
Publication history
November 01, 2001

Abstract

High-temperature-resistant polymers are used in aerospace, electronic, and other applications that demand outstanding elevated-temperature physical and mechanical properties. This article discusses the general characteristics of condensation-type polyimides and polymerization of monomer reactants (PMR) polyimides. It provides information on the applications of PMR-15 with illustrations.

You do not currently have access to this content.
Don't already have an account? Register

Tito T. Serafini, Stephen C. Mitchell, 2001. "High-Temperature Applications", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal