Prepreg hand lay-up process is versatile, reliable, cost-effective, and high quality process for fabricating large or small components. This article discusses the technique characteristics and applications of prepreg hand lay-up process. It describes the stages involved in the process of lay-up, namely, lay-up definition, ply-kit cutting, layup, debulking, and preparation for curing. The article concludes with a discussion on the component properties and design guidelines of the prepreg hand lay-up process.