Affordability is the key issue facing design engineers and manufacturers of composite components for current and next-generation aircraft, spacecraft, propulsion systems, and other advanced applications. This article describes software tools available for modeling and analyzing costs associated with design and manufacturing options for advanced composites programs. It presents an example of a composite exhaust nozzle shroud where the design and manufacture options were analyzed and adjusted, based on the use of cost analysis tools. The article also lists some of the attributes found in various cost modeling software and the potential cost benefits.