This article describes the synthesis, manufacturing, and properties of both the neat soy-based resins and the glass, flax, and hemp composites. A tabulation of fatty-acid distribution in various plant oils is provided. The article discusses synthetic pathways for triglyceride-based monomers and provides a discussion on acrylated epoxidized soybean oils (AESO), maleinized soyoil monoglyceride (SOMG/ MA), maleinized hydroxylated oil (HO/MA). The polymer properties of the AESO, SOMG/MA, and HO/MA are also discussed. The article describes ballistic impact resistance of soy resin composites and concludes with a discussion on biodegradable composites.