This article focuses on the design process, materials, and manufacturing techniques for one-off and low-volume production sailing craft. These include racing yachts of typically 10 to 20 m length for short coastal events, 20 to 25 m ocean racers, 24 m America's Cup racing craft, multihull racers of 35 m or more, and large luxury cruising craft. The article discusses tooling, laminating practice, curing, mold removal, and quality control, for manufacturing hulls, decks, masts, and appendages using composites.