Abstract

Cyanate ester resins are a family of high-temperature thermosetting resins that bridge the gap in thermal performance between engineering epoxy and high-temperature polyimides. This article discusses the chemistry, properties and characteristics of the cyanate ester resins. It describes the processing procedures for the cyanate ester resins and provides information on properties for selected applications, such as space applications, radomes, and printed circuit boards.