This article describes the characteristics of thermoplastic composites and its material forms. It presents the steps and considerations in manufacturing the thermoplastic composites. The article provides a description of various techniques of manufacturing, such as consolidation, autoclave molding, diaphragm forming, compression molding, roll forming, bladder molding, liquid molding, filament winding, and pultrusion.