Abstract

Designing composites for structural performance initially involves meeting a set of desired performance specifications at a minimum cost. This article discusses the factors that are considered in design for manufacturing of polymeric composites. It describes the various aspects of manufacturing, forming process, and post-processing and fabrication for designing the composites.