This article discusses the advantages of polymer matrix composite for automotive application in terms of design drivers, noise, vibration, harshness efficiency, process materials property constraints, safety and reliability, design optimization, structural and appearance requirements, recyclability, and processability. It describes the properties of high-volume composites used in automotive industries. The article provides a discussion on state-of-the-art and developing technologies in automotive field.