Abstract

This article provides a summary of the concepts discussed in the articles under the section “Failure Analysis” in ASM Handbook, Volume 21: Composites. Most of the information in this section is geared toward organic-matrix composites, although there is some information on failure analysis and fractography of ceramic- and metal-matrix composites.