Abstract

This article begins with a discussion on driving forces for recycling of composites. It reviews the recycling process of thermoset-matrix composites and thermoplastic-matrix composites. The recycling of thermoset-matrix composites includes regrind, chemical, energy recovery, and thermal processes. Thermoplastic-matrix composites are recycled by regrinding, compounding/blending and reprocessing. The article concludes with discussion on the properties of recycled composite fibers.

You do not currently have access to this chapter.
Don't already have an account? Register

John M. Henshaw, 2001. "Recycling and Disposal of Polymer-Matrix Composites", Composites, Daniel B. Miracle, Steven L. Donaldson