Abstract

This article presents the importance of progressing from post-manufacturing inspection/verification to in-process inspection/verification methods. It lists various quality assurance factors considered for typical composite laminate lay-up process. The article provides information on composite cure tooling that is fabricated from steel, aluminum, or high-temperature composite materials. The quality assurance for commercial applications is reviewed. The article concludes with a discussion on the data fusion systems that are designed to provide nondestructive analysis data from fabrication and assembly processes for each individual composite part.

You do not currently have access to this chapter.
Don't already have an account? Register

Grover Aaron Henson, III, 2001. "Introduction to Quality Assurance", Composites, Daniel B. Miracle, Steven L. Donaldson