Vacuum infusion is a resin injection technique derived from resin transfer molding. This article discusses the characteristics of the technique and its applications. It presents the theory and background of the technique and provides an illustration of how parts are made. The article provides information on equipment and material used for vacuum infusion. It describes the mechanical properties of components and summarizes the influence of production on the properties. The article concludes with a discussion on design guidelines.