Introduction to Post-Processing and Assembly
By
Flake C. Campbell
Flake C. Campbell
The Boeing Company
Search for other works by this author on:
-
Published:2001
Publication history
November 01, 2001
Abstract
This article provides a summary of the concepts discussed in the articles under the Section “Post-Processing and Assembly” ASM Handbook, Volume 21: Composites.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Flake C. Campbell, Introduction to Post-Processing and Assembly, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 615, https://doi.org/10.31399/asm.hb.v21.a0003423
Download citation file:
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.
Related Book Content
Guide to Materials Selection
Engineered Materials Handbook Desk Edition
Ceramic-Matrix Composites
Lightweight Materials Understanding the Basics
Ceramic-Matrix Composites
Engineered Materials Handbook Desk Edition
Polymer-Matrix Composites
Lightweight Materials Understanding the Basics
Introduction to Polymer-Matrix Composites
Engineered Materials Handbook Desk Edition
Joining and Assembly of Polymer-Matrix Composites
Engineered Materials Handbook Desk Edition
Machining, Drilling, and Cutting of Polymer-Matrix Composites
Engineered Materials Handbook Desk Edition
Fatigue Fracture Appearances
Failure Analysis and Prevention
Nondestructive Testing of Composites (Polymer- and Metal-Matrix Composites)
Nondestructive Evaluation of Materials
Forging of Discontinuously Reinforced Aluminum Composites
Metalworking: Bulk Forming