Engineering Mechanics and Analysis of Metal-Matrix Composites
-
Published:2001
Abstract
The goal of micromechanics and analysis is to use the predictive methodology to develop tailored composites and also to make accurate predictions of their performance in service. This article reviews results derived from micromechanics analyses, based on finite-element method of unidirectional fiber reinforced metal matrix composites (MMCs). It discusses the elastic deformation and elastic-plastic deformation analysis of discontinuously reinforced MMCs. The article provides an overview of analysis of strength, fatigue, and fracture toughness for macromechanics fiber-reinforced and discontinuous reinforced composites.
Sign in
ASM members
Member Sign InBhaskar S. Majumdar, Engineering Mechanics and Analysis of Metal-Matrix Composites, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 396–406, https://doi.org/10.31399/asm.hb.v21.a0003399
Download citation file:
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.