Abstract
This article provides a summary of the concepts discussed in the articles under the section “Failure Analysis” in ASM Handbook, Volume 21: Composites. Most of the information in this section is geared toward organic-matrix composites, although there is some information on failure analysis and fractography of ceramic- and metal-matrix composites.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Patricia L. Stumpff, Introduction to Failure Analysis, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 949–950, https://doi.org/10.31399/asm.hb.v21.a0003460
Download citation file:
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.
Related Book Content
Ceramic-Matrix Composites
Lightweight Materials Understanding the Basics
Ceramic-Matrix Composites
Engineered Materials Handbook Desk Edition
Metal-Matrix Composites
Lightweight Materials Understanding the Basics
Forging of Discontinuously Reinforced Aluminum Composites
Metalworking: Bulk Forming
Heat Treating of Magnesium Alloy Metal-Matrix Composites
Heat Treating of Nonferrous Alloys
Metal-Matrix Composites: Atlas of Fractographs
Fractography
Guide to Materials Selection
Engineered Materials Handbook Desk Edition
Metal-Matrix Composites
Metals Handbook Desk Edition, 2nd Ed. (2nd Edition)
Foundry Practice for Nonferrous Alloys
Metals Handbook Desk Edition, 2nd Ed. (2nd Edition)
Acoustic Emission Inspection
Nondestructive Evaluation of Materials